Internal Oxidation for Piping Welds Webinar

Internal Oxidation for Piping Welds Webinar

When welding stainless steel and nickel alloy piping using an open root or consumable insert, the root side of the joint (i.e., the inside surface of the pipe at a weld) must be protected from the oxygen in the atmosphere, otherwise the liquid weld metal will oxidize badly creating a surface that is not only discolored but is also quite rough. This roughness and discoloration will reduce the corrosion resistance of the metal at the weld. In this webinar you will learn what is acceptable level of discoloration of the root side of the stainless-steel pipe weld and provides general guidance on the level of root surface discoloration that can be tolerated for some service conditions.